What Is “Hesitant Flow” in Injection Molding? A Simple Explanation of Causes, Defects, and Countermeasures
Introduction
Have you ever struggled with defects in injection molding, such as “only thin ribs failing to fill” or “short shots occurring near the gate”? Even when wall thickness and resin temperature seem to be within acceptable ranges, specific areas simply won’t mold properly. One cause that’s often overlooked is “hesitant flow.”

In this article, we’ll provide a clear explanation—tailored for those involved in product and mold design—of what hesitant flow is, why it occurs, what types of defects it causes, and how to address it.
What Is Hesitation Flow?
Hesitation flow is a phenomenon in which, as molten resin fills the mold cavity, the flow into areas where it is difficult to flow—such as thin-walled sections—temporarily stops or slows down significantly. It is called “hesitation” in English because the resin appears to be “hesitating” to move forward.

Plastic has the property of flowing preferentially along paths of least resistance, just as water flows to lower elevations. In products that combine thick-walled and thin-walled sections, the plastic first flows into the thick-walled sections, where flow is easier, and then hesitates at the entrance to the thin-walled sections. The fundamental problem with hesitation flow is that the plastic cools during this “hesitation period.”
The Mechanism Behind Hesitant Flow
Hesitant flow occurs due to the combination of two factors: “differences in flow resistance” and “cooling by the mold.” A typical flow sequence is as follows:
Resin reaches the branching point: The leading edge of the resin flow reaches the branching point between the thick-walled and thin-walled sections.
The path of easier flow is prioritized: Since flow resistance increases more sharply as wall thickness decreases, the resin flows preferentially into the thick-walled section and makes little progress at the entrance to the thin-walled section.
Resin cools during stagnation: The resin stagnating at the entrance to the thin-walled section loses heat to the mold, causing its temperature to drop. As the temperature drops, viscosity increases, creating a vicious cycle in which flow becomes even more difficult. A solidified layer also forms on the surface, further narrowing the flow path.
Delayed flow or solidification: Once the thick-walled section is filled and pressure rises, the resin finally begins to flow into the thin-walled section. However, if the resin has already cooled by that point, it will solidify before reaching the tip of the thin-walled section.
The likelihood of this phenomenon occurring varies depending on the type of resin. Crystalline resins such as POM, PA, and PP tend to be susceptible to hesitation flow because solidification progresses rapidly once the temperature falls below a certain point. Additionally, high-viscosity materials, such as glass-fiber-reinforced composites, require significant pressure to flow into thin-walled sections, so caution is necessary.
Shapes and Locations Prone to Occurrence
Hesitation flow is more likely to occur in the following shapes and locations:
・Thin ribs or bosses branching off from thick-walled sections: Thin-walled sections that branch off from the main flow path—such as reinforcing ribs, positioning protrusions, and thin flanges—are typical locations where this phenomenon occurs.
・Thin-walled sections near the gate: Although it may seem counterintuitive, the closer a section is to the gate, the greater the risk. Since the resin reaches the entrance of the thin-walled section at an early stage, there is a longer waiting period before the entire part is filled and the pressure rises.
・Geometries where thin-walled sections end in a dead end: Gas has nowhere to escape, and back pressure makes it even harder for resin to flow in.
・Hinge areas and extremely thin-walled sections: Areas where wall thickness is significantly reduced, such as in one-piece hinges, experience extremely high flow resistance.
Molding Defects Caused by Hesitant Flow
Hesitant flow causes the following molding defects:
Short shot (incomplete filling): This is the most common defect. The resin solidifies while stagnant, preventing it from filling all the way to the tip of the thin-walled section. It is characterized by its instability in mass production, as it may or may not occur depending on even slight changes in conditions.
[Verification Experiment] What happens when continuous molding is performed using a mold without gas vents?
Appearance Defects: As cooled resin flows in slowly, flow marks, uneven gloss, pitting, and poor surface texture reproduction occur. This poses a significant problem in terms of product aesthetics.
Reduced Strength: When cooled, high-viscosity resin flows in, causing uneven molecular orientation and residual stress. The impact on functionality—such as increased susceptibility to cracking at the bases of ribs and bosses—cannot be ignored.
Dimensional Variation: Since sufficient pressure is not transmitted to thin-walled areas, shrinkage increases, leading to unstable dimensions.
Countermeasures for Hesitant Flow
Countermeasures for hesitant flow boil down to two points: “Do not let the resin wait at the inlet to thin-walled areas” and “Do not allow it to cool while waiting.” The most effective measures are taken during the upstream stages of product and mold design; there are limits to what can be achieved through molding conditions alone.
Stages of Response | Key Measures | Objectives |
Product Design | Position the thin-walled section closer to the trailing edge of the flow. | Reduce dwell time |
Ensure the ribs of the boss have sufficient thickness and make the transition in thickness gradual | Minimize the difference in flow resistance | |
Mold Design | Adjust the gate position so that the flow enters the thin-walled section directly and more quickly. | Change the priority of the flow |
Revision of Gate Scores, Addition of Gas Vents | Improved filling balance, reduced back pressure | |
Molding Conditions | Increase the injection speed | Shorten the cooling time during the stagnation phase |
Increase the resin temperature and mold temperature | Delay setting | |
Materials | Select a grade with high fluidity | To facilitate flow into the thin-walled section |
One point to note here is the side effects of countermeasures based on molding conditions. Increasing the injection speed or temperature can lead to issues such as flash, burn marks, and longer cycle times. Attempting to resolve these issues solely through condition adjustments narrows the molding condition range (process window), compromising stability during mass production. To achieve a fundamental solution, countermeasures implemented during the design phase are essential.
Preliminary Verification via Flow Analysis (CAE)
Hesitation flow can be predicted using resin flow analysis before the mold is manufactured. There are three key points to check:
Filling animation: Check for any areas where the flow front temporarily stops or progresses extremely slowly.
Flow front temperature: Check whether the temperature drops significantly in localized areas at the entrance or tip of thin-walled sections.
Comparison of Filling Patterns: Compare multiple designs with different gate locations and wall thicknesses to verify whether stagnation is resolved.
Note that flow hesitation is greatly influenced by the resin’s viscosity characteristics and solidification temperature; therefore, even for the same product geometry, changing the material will yield different results. It is crucial to use material data for the specific grade that will actually be used in the analysis.
Simple Flow Analysis App: Techshop.sim
Summary
Hesitation flow is a phenomenon in which stagnation occurs at the entrance of thin-walled sections because the resin prioritizes paths where it flows more easily; during this time, the resin cools and becomes harder to flow. This can cause short shots, cosmetic defects, and reduced strength, and is particularly likely to occur with crystalline resins, high-viscosity materials, and in thin-walled sections near the gate.
Since there are limits to addressing this issue through molding condition adjustments alone, utilizing flow analysis during the product and mold design stages to evaluate the placement of thin-walled sections and gate locations is the surest path to stable mass production. If you are experiencing defects such as “only specific ribs not being filled,” why not consider the possibility of hesitation flow?






Comments