One of the most common molding defects seen in injection molding operations is “stringing.”


When stringing occurs, it can lead to various problems, such as:

・Resin residue adhering to the molded part

・Resin adhering to the mold

・Appearance defects around the gate

・Increased mold cleaning frequency

・Conveyor issues during automated molding

・Foreign matter entering the mold’s mating surfaces, leading to clamping failures


and more.


In this article, we will provide a clear explanation of why “stringing” occurs in injection molding, along with its causes and countermeasures.


1. What Is Stringing?


Stringing is a phenomenon in which molten resin is drawn out in thin, thread-like strands from the nozzle of an injection molding machine or the gate of a mold.


It can occur when the injection cycle ends and the mold opens, or when the nozzle is withdrawn from the mold.


Visually, it is similar to the “stretchy” strands that form when you pull on hot cheese.

ピザのチーズのイメージ

Because molten resin is viscous, if it is pulled before it has fully solidified, it will stretch rather than break.


2. Why Does Stringiness Occur?


Simply put, the main cause of stringiness is that

“the resin has not fully solidified.”


In injection molding, resin pellets are heated and melted, then injected into a mold.


The resin is then cooled and solidified inside the mold.


However, if the resin near the nozzle tip or around the gate is still soft and the mold or nozzle moves, the resin is pulled, causing stringing, or drips due to gravity.


糸引きが発生するメカニズム

Therefore, the causes can be broadly categorized as follows:


① The resin temperature is too high

② The resin pressure is too high

③ The resin has not solidified sufficiently

④ There is a problem with the nozzle or mold design

⑤ The properties of the resin itself

and so on.


3. Cause ①: The resin temperature is too high


One of the most obvious causes is an increase in resin temperature.


Generally, as the temperature of a resin increases, its viscosity decreases, making it flow more easily.

For example, if you compare cold oil to heated oil, the heated oil is thinner and flows more easily.

Similarly, as the temperature of a resin rises, its fluidity increases.

As a result, the resin at the tip of the nozzle is more likely to drip, or the resin may form strings as the nozzle pulls away from the mold.


Countermeasures


First, check the following:

Cylinder temperature

Nozzle temperature

Mold temperature

Actual resin temperature


and so on.


However, simply lowering the temperature is not always the solution.


If the temperature is lowered too much, it may lead to other molding defects such as underfill, weld lines, or increased pressure.


Therefore, it is important to optimize the temperature within the range suitable for molding.


4. Cause 2: Excessive Injection Pressure or Holding Pressure


In injection molding, the screw forces molten resin into the mold.

At this point, high pressure is applied to the resin.

If pressure remains near the nozzle even after molding is complete, that pressure may force resin out from the nozzle tip.

This can be considered residual pressure.


For example, if you remove the cap from a syringe while pressing down on the tip, the liquid inside will squirt out.


Similarly, in an injection molding machine, if force remains inside the nozzle to push the resin out, resin may leak out after the injection cycle is complete.


Countermeasures


・Do not set the holding pressure higher than necessary

・Optimize the holding time

・Check the screw position after the injection cycle is complete

・Adjust the suck-back amount


These are some of the methods available.

5. Cause 3: Inappropriate Sackback Amount


Sackback is a crucial measure for preventing stringing.

Sackback refers to the action of retracting the screw slightly after injection is complete.

Retracting the screw relieves the pressure of the resin trying to push toward the nozzle tip, thereby preventing the resin from coming out of the nozzle.


Think of it like squeezing a tube of toothpaste slightly and then pulling back a little to release the pressure at the tip.


If the retraction amount is too small, pressure remains inside the nozzle, making it more likely for drips or stringing to occur.

On the other hand, if the retraction amount is too large, air may become entrapped in the resin, or stability during metering may deteriorate.


Therefore,


“More is not necessarily better.”


You need to set the appropriate value based on the resin and molding conditions.


6. Cause 4: Nozzle Shape and Compatibility with the Mold


Stringiness is influenced not only by molding conditions but also by the structure of the nozzle and mold.


For example, if the nozzle tip is shaped in a way that causes resin to accumulate easily, the resin remaining after injection can cause stringiness.


Additionally, if the contact between the nozzle and the mold is not proper, resin leakage may occur.


Therefore,

・Nozzle tip shape

・Contact between the nozzle and the sprue bushing

・Nozzle radius (R)

・Sprue shape

・Gate shape


It is also important to check these factors.


In particular, if stringing suddenly occurs after a mold change, checking the mold itself—not just the molding conditions—will make it easier to identify the cause.


7. Cause 5: Differences Based on Resin Type


The likelihood of stringing occurring varies depending on the resin.

This is because each resin differs in terms of:

・Viscosity

・Melting temperature

・Ease of solidification upon cooling

・Elasticity

・Flowability


and other factors.


For example, resins with low viscosity that flow easily may tend to drip from the nozzle under certain conditions.


Additionally, resins containing fillers such as glass fibers may exhibit flow characteristics different from those of standard resins.


Therefore,


it is not necessarily true that “since there were no issues with a different resin, these conditions will work here as well.”


When changing resins, it is important to reconfirm the appropriate temperature, pressure, and suck-back conditions.


8. Checkpoints When Stringing or Dripping Occurs

In actual molding operations, it is important to isolate the causes one by one.

For example, it is advisable to check in the following order:


STEP 1: Check the Resin Temperature


Check whether the set temperature is too high.

In particular, check whether the nozzle temperature is too high.


STEP 2: Check Molding Conditions


Check the injection pressure, holding pressure, and holding time.

Verify that the pressure is not set higher than necessary.


STEP 3: Check the Sackback


Check whether the sackback volume is too low.

Adjust it gradually and check whether the stringing and sagging improve.


STEP 4: Check the Nozzle and Mold


Check whether resin has accumulated on the nozzle tip, sprue bushing, or around the gate.

STEP 5: Check the Resin


If the issue occurred after changing resins, check for differences in resin flowability or molding temperature.


9. Simply “Lowering the Temperature” Won’t Solve the Problem


When stringing occurs,you might think,


“Let’s just try lowering the temperature for now.”


Of course, adjusting the temperature is one effective countermeasure, but if you lower it too much,

insufficient filling → insufficient holding pressure → reduced weld strength → cosmetic defects

and other problems may arise.


The key is


not just to eliminate stringing, but to address the root cause while maintaining the overall quality of the molded part.


For example,

“Slightly lower the resin temperature,”

“Optimize the suckback,”

“Review the holding pressure conditions,”

“Check the nozzle and sprue geometry,”


and so on—we combine multiple factors to find the optimal conditions.


10. Summary


“Stringing” in injection molding occurs when molten resin around the nozzle or gate stretches or drips before it solidifies.


The main causes include:

・Resin temperature is too high

・Injection pressure or holding pressure is too high

・Residual pressure remains inside the nozzle

・The suckback volume is inappropriate

・Problems with the nozzle or sprue geometry

・Flow characteristics of the resin itself


are among the possible causes.


It is particularly important to


consider the issue from the perspective of


“Why is the resin coming out of the nozzle?”


Organizing the causes from the four perspectives of “temperature,” “pressure,” “solidification,” and “shape” makes it easier to isolate the problem.


Furthermore, stringing is not merely a cosmetic defect.


When resin residue adheres to the mold, it increases the burden of mold maintenance. On automated molding lines, adhered resin can affect products and equipment, potentially reducing molding stability.


Therefore, when stringing occurs, rather than simply “wiping off the resin,”


it is important to ask, “Why is the resin stringing?”


and identify the cause by examining molding conditions, materials, and mold design.



Comments

Rated 0 out of 5 stars.
No ratings yet

Add a rating

Concerns about plastics
Did you solve?

You can find the desired content from the
top page content from the top page.

23989485.png

★月間アクセスランキング★

bottom of page